Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 251 °C | 484 °F | ASTM D648 |
Ensinger Tecatron® XP-61L Compression Molded PPS Compound, 25% Fiberglass and Mineral Filled Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |