Polymer Property : Heat Distortion Temperature = 93.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat Distortion Temperature 93.0 °C
199 °F
ISO 75A
Lucite International Diakon® TD510 Toughened Acrylic Compound
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by..