Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 95.0 - 119 °C | 203 - 246 °F | Average value: 108 °C Grade Count:6 |
Overview of materials for Polypropylene, Fiber Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app.. |
|||
Heat Distortion Temperature | 95.0 °C | 203 °F | ISO 75/B |
Iran Petrochemical (PCC) V 30 S Polypropylene V 30 S is a high fluidity PP for the protection of staple fibers with improved thermo bonding ability for no woven fabrics.Application: the typical application of this grade are cover stock for diap.. |
|||
Heat Distortion Temperature | 95.0 °C | 203 °F | |
Atom Adhesives AA-CARB 61 Epoxy Adhesive AA-CARB 61 is an epoxy adhesive and coating formulation based on conductive carbon. AA-CARB 61 is recommended for electronic bonding and sealing applications that require both fine electrical and me.. |
|||
Heat Distortion Temperature | 95.0 °C | 203 °F | Cured |
Atom Adhesives AA-DUCT 902 Epoxy Adhesive and Coating AA-DUCT 902 is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value of.. |