Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Vaporization | 117.2 J/g | 50.43 BTU/lb | |
3M Novec™ 7200DL Engineered Fluid A high-purity version of 3M™ Novec™ 7200, 3M™ Novec™ 7200DL is tightly-controlled for ions, metals and non-volatile residue. It is used when an application calls for high-purity materials, or a .. |