Polymer Property : Heat of Vaporization = 201.0 J/g Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat of Vaporization 201.0 J/g
86.45 BTU/lb
3M Novec™ 71DE Engineered Fluid
3M™ Novec™ 71DE is an azeotrope containing 3M™ Novec™ 7100 and 1,2 trans-dichloroethylene. It maintains a constant liquid and vapor composition at its boiling point. It can be used in many mediu..