Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Vaporization | 246 J/g | 106 BTU/lb | |
Enviro Tech International EnSolv® n-Propyl Bromide Vapor Degreasing Solvent EnSolv is the perfect direct replacement for TCE, Perchloroethylene, 1,1,1-Trichloroethane and other hazardous vapor degreasing and general use solvents for critical applications such as oxygen serv.. |