Polymer Property : Heat of Vaporization = 39.6 BTU/lb Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat of Vaporization 92.0 J/g

@Temperature 55.0 °C
39.6 BTU/lb

@Temperature 131 °F
at boiling point
Solvay Specialty Polymers Galden® HT55 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..
Heat of Vaporization 92.0 J/g

@Temperature 55.0 °C
39.6 BTU/lb

@Temperature 131 °F
at boiling point
Solvay Specialty Polymers Galden® SV55 PFPE Solvent
Galden® SV grades are specifically recommended for use as solvents.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service temperature..