Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.618 J/g-°C @Temperature 900 °C |
0.148 BTU/lb-°F @Temperature 1650 °F |
|
Special Metals INCOLOY® alloy 832 Stainless Steel INCOLOY® alloy 832 is a low cost stainless steel developed specifically for domestic and industrial sheathed heater applications. With specific chemistry additions to ensure satisfactory formula.. |
|||
Specific Heat Capacity | 0.620 J/g-°C @Temperature 20.0 - 500 °C |
0.148 BTU/lb-°F @Temperature 68.0 - 932 °F |
|
ATI Allegheny Ludlum AL 4565™ Corrosion Resistant Stainless Steel Characteristics:Very high resistance to pitting and crevice corrosion Excellent general corrosion resistance in a variety of media Higher mechanical propertied then conventional stainless steels Go.. |