Thermal Properties Metric English Comments
Specific Heat Capacity 0.741 J/g-°C

@Temperature 23.0 °C
0.177 BTU/lb-°F

@Temperature 73.4 °F
Zoltek Panex 35® Carbon Felt
Carbon FeltApplications include: Thermal, Corrosive, or Conductive applications