Thermal Properties Metric English Comments
Specific Heat Capacity 0.795 J/g-°C

@Temperature 600 °C
0.190 BTU/lb-°F

@Temperature 1110 °F
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel
BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303..