Thermal Properties Metric English Comments
Specific Heat Capacity 1.26 J/g-°C

@Temperature 50.0 °C
0.301 BTU/lb-°F

@Temperature 122 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic..
Specific Heat Capacity 1.26 J/g-°C

@Temperature 50.0 °C
0.301 BTU/lb-°F

@Temperature 122 °F
ASTM C351
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber
AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch..