Thermal Properties Metric English Comments
Specific Heat Capacity 1.35 J/g-°C

@Temperature 50.0 °C
0.323 BTU/lb-°F

@Temperature 122 °F
DSC
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro..
Specific Heat Capacity 1.35 J/g-°C

@Temperature 50.0 °C
0.323 BTU/lb-°F

@Temperature 122 °F
DSC
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation..
Specific Heat Capacity 1.35 J/g-°C

@Temperature 50.0 °C
0.323 BTU/lb-°F

@Temperature 122 °F
ASTM C351
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621..
Specific Heat Capacity 1.35 J/g-°C

@Temperature 50.0 °C
0.323 BTU/lb-°F

@Temperature 122 °F
ASTM C351
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula..
Specific Heat Capacity 1.35 J/g-°C

@Temperature 50.0 °C
0.323 BTU/lb-°F

@Temperature 122 °F
ASTM C351
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and..
Specific Heat Capacity 1.35 J/g-°C

@Temperature 50.0 °C
0.323 BTU/lb-°F

@Temperature 122 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr..