Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.51 J/g-°C @Temperature 60.0 °C |
0.361 BTU/lb-°F @Temperature 140 °F |
|
LG Chemical BPA Structure & Characteristics: (CH3)2C(C6H4OH)2 . BPA is an us powder with white colorOverview: Bisphenol-A(BPA) is used primarily to make polycarbonate and epoxy resins, both of which are used in a w.. |