Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.375 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.57 J/g-°C

@Temperature 20.0 °C
0.375 BTU/lb-°F

@Temperature 68.0 °F
Dow SPECFLEX™ NC 700 Polyol
SPECFLEX™ NC 700 polyol is a unique grafted polyether polyol containing copolymerized styrene and acrylonitrile. It is manufactured without the use of BHT and has been filtered to 200 microns. CA..
Copyright © lookpolymers.com All Rights Reserved