Thermal Properties Metric English Comments
Specific Heat Capacity 0.450 J/g-°C

@Temperature 25.0 °C
0.108 BTU/lb-°F

@Temperature 77.0 °F
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Specific Heat Capacity 0.450 J/g-°C

@Temperature 25.0 °C
0.108 BTU/lb-°F

@Temperature 77.0 °F
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Specific Heat Capacity 0.450 J/g-°C

@Temperature 25.0 °C
0.108 BTU/lb-°F

@Temperature 77.0 °F
Haynes Hastelloy® G-35® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Specific Heat Capacity 0.450 J/g-°C

@Temperature 25.0 °C
0.108 BTU/lb-°F

@Temperature 77.0 °F
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Specific Heat Capacity 0.450 J/g-°C

@Temperature 20.0 - 100 °C
0.108 BTU/lb-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum AL 4565™ Corrosion Resistant Stainless Steel
Characteristics:Very high resistance to pitting and crevice corrosion Excellent general corrosion resistance in a variety of media Higher mechanical propertied then conventional stainless steels Go..
Specific Heat Capacity 0.450 J/g-°C

@Temperature 25.0 °C
0.108 BTU/lb-°F

@Temperature 77.0 °F
Haynes Hastelloy® G-35® Nickel Alloy Sheet, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..
Specific Heat Capacity 0.450 J/g-°C

@Temperature 25.0 °C
0.108 BTU/lb-°F

@Temperature 77.0 °F
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..
Specific Heat Capacity 0.450 J/g-°C

@Temperature 25.0 °C
0.108 BTU/lb-°F

@Temperature 77.0 °F
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..