Polymer Property : Specific Heat Capacity = 0.461 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.93 J/g-°C

@Temperature 200 °C
0.461 BTU/lb-°F

@Temperature 392 °F
DSC
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist..
Specific Heat Capacity 1.93 J/g-°C

@Temperature 200 °C
0.461 BTU/lb-°F

@Temperature 392 °F
ASTM C351
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
KetaSpire® KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire® PEEK is produced to the highest industry standards and is characterized b..
Specific Heat Capacity 1.93 J/g-°C

@Temperature 200 °C
0.461 BTU/lb-°F

@Temperature 392 °F
ASTM C351
Solvay Specialty Polymers KetaSpire® KT-880FP Polyetheretherketone (PEEK)
KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from th..
Specific Heat Capacity 1.93 J/g-°C

@Temperature 20.0 °C
0.461 BTU/lb-°F

@Temperature 68.0 °F
Dow VORANOL™ 4703 Polyether Polyol
VORANOL™ 4703 polyether polyol is a nominal 5000 molecular weight, high reactivity capped triol. It has a high primary hydroxyl content making it suitable for use in making all types of high resil..