Polymer Property : Specific Heat Capacity = 0.470 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.97 J/g-°C

@Temperature 37.8 °C
0.470 BTU/lb-°F

@Temperature 100 °F
Paratherm Corporation Paratherm™ HR™ Heat Transfer Fluid
Paratherm HR™ Heat Transfer Fluid is an alkylated-aromatic based heat transfer fluid formulated for closed loop liquid phase heating to 650°F in fired heaters and 675°F in waste heat recovery and..
Specific Heat Capacity 1.97 J/g-°C

@Temperature 200 °C
0.470 BTU/lb-°F

@Temperature 392 °F
DSC
Eastman Cadence™ GS1 Copolyester for film calendering
Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe..
Specific Heat Capacity 1.97 J/g-°C

@Temperature 200 °C
0.470 BTU/lb-°F

@Temperature 392 °F
DSC
Eastman Cadence™ GS2 Copolyester for film calendering
Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe..
Specific Heat Capacity 1.97 J/g-°C

@Temperature 200 °C
0.470 BTU/lb-°F

@Temperature 392 °F
DSC
Eastman Cadence™ GS3 Copolyester for film calendering
Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe..
Specific Heat Capacity 1.97 J/g-°C

@Temperature 200 °C
0.470 BTU/lb-°F

@Temperature 392 °F
DSC
Eastman Cadence™ GS4 Copolyester for film calendering
Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe..
Specific Heat Capacity 1.97 J/g-°C

@Temperature 37.8 °C
0.470 BTU/lb-°F

@Temperature 100 °F
Duratherm 600 Paraffinic Heat Transfer Fluid
Duratherm 600 - thermal fluid rated to 600°F it contains the industries most aggressive blend of additives for long, trouble free operation in a variety of applications. Specifically engineered to ..
Specific Heat Capacity 1.97 J/g-°C

@Temperature 37.8 °C
0.470 BTU/lb-°F

@Temperature 100 °F
Duratherm G Polyalkylenev Glycol Heat Transfer Fluid
Glycol fluids such as Ucon 500(TM) have been used for years but have, until now offered very little protection from negative elements such as oxidation. Duratherm G also has reduced odors and improv..