Thermal Properties Metric English Comments
Specific Heat Capacity 0.510 J/g-°C

@Temperature 300 °C
0.122 BTU/lb-°F

@Temperature 572 °F
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Specific Heat Capacity 0.510 J/g-°C

@Temperature 300 °C
0.122 BTU/lb-°F

@Temperature 572 °F
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Specific Heat Capacity 0.510 J/g-°C

@Temperature 300 °C
0.122 BTU/lb-°F

@Temperature 572 °F
Haynes Hastelloy® G-35® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Specific Heat Capacity 0.510 J/g-°C

@Temperature 300 °C
0.122 BTU/lb-°F

@Temperature 572 °F
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Specific Heat Capacity 0.510 J/g-°C

@Temperature 300 °C
0.122 BTU/lb-°F

@Temperature 572 °F
Haynes Hastelloy® G-35® Nickel Alloy Sheet, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..
Specific Heat Capacity 0.510 J/g-°C

@Temperature 300 °C
0.122 BTU/lb-°F

@Temperature 572 °F
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..
Specific Heat Capacity 0.510 J/g-°C

@Temperature 300 °C
0.122 BTU/lb-°F

@Temperature 572 °F
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..