Polymer Property : Specific Heat Capacity = 0.529 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.529 J/g-°C

@Temperature 200 °C
0.126 BTU/lb-°F

@Temperature 392 °F
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel
BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303..