Thermal Properties Metric English Comments
Specific Heat Capacity 0.612 J/g-°C

@Temperature 500 °C
0.146 BTU/lb-°F

@Temperature 932 °F
International Mold Steel Daido DRM3 Matrix High-Speed Steel
This conventional grade MH88 has been improved to DRM3. High hardness and tough DRM3 with excellent hardenability is suitable for high precision cold working tools.Information provided by Internatio..