Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.627 J/g-°C @Temperature 700 °C |
0.150 BTU/lb-°F @Temperature 1290 °F |
|
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy NIMONIC® alloy 91 is a wrought nickel-chromium-cobalt based alloy strengthened by additions of aluminum and titanium.This alloy is a modification of NIMONIC alloy 90, but has an increased chromium .. |