Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.21 J/g-°C @Temperature 80.0 °C |
0.290 BTU/lb-°F @Temperature 176 °F |
ASTM E1269 |
DAK Americas Laser+® MB912 PET Product Description: Laser+® MB912 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. It delivers fast, efficient pr.. |
|||
Specific Heat Capacity | 1.21 J/g-°C @Temperature 80.0 °C |
0.289 BTU/lb-°F @Temperature 176 °F |
|
3M Novec™ 7500 Engineered Fluid 3M™ Novec™ 7500 is a non-flammable fluid with a very low global warming potential (GWP.) Its' excellent inerting and dielectric properties make it a viable replacement for higher GWP fluids such a.. |