Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.64 J/g-°C @Temperature 218 °C |
0.630 BTU/lb-°F @Temperature 425 °F |
|
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid Paratherm CR® heat transfer fluid is a blend of synthetic components formulated to provide superior cooling performance in closed-loop heat-transfer systems operating down to -88°C (-127°F) yet i.. |
|||
Specific Heat Capacity | 2.64 J/g-°C @Temperature 204 °C |
0.630 BTU/lb-°F @Temperature 400 °F |
|
Duratherm 450 Paraffinic Heat Transfer Fluid Duratherm 450 - thermal fluid specifically engineered for applications requiring process heating and cooling efficiently between 30°F and 450°F. Economical and thermally stable, Duratherm 450 offe.. |