Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Vyram™ 9201-85 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Processing Temperature | 190 - 230 °C | 374 - 446 °F | |
PolyChem Alloy FlexGel 5007HF TPE A Zero Shore Hardness TPE, FlexGel is soft, flexible, and resilient, with excellent chemical and moisture resistance. The material can be decorated, printed, reground, and reprocessed without any si.. |
|||
Processing Temperature | 170 - 230 °C | 338 - 446 °F | |
PolyChem Alloy PolyBlaz 7525PM An Antimicrobial Agent Masterbatch. |
|||
Processing Temperature | 200 - 230 °C | 392 - 446 °F | Barrel Temperature |
SABIC PP 651H Polypropylene Random Copolymer for PIPE Product Description: PP 651H is specially designed for transport of hot and cold drinking water. This grade is highly heat stabilized and specially formulated for extraction resistance.Typical App.. |
|||
Processing Temperature | 180 - 230 °C | 356 - 446 °F | |
LG Chemical LUTENE-H FE0070 HDPE LUTENE-H FE0070 is mainly intended for the extrusion of blown film with high mechanical properties for the manufacture of "T-Shirt" grocery sacks, can liners. Especially, LUTENE-H FE0070 resin can b.. |
|||
Processing Temperature | 180 - 230 °C | 356 - 446 °F | |
IRPC Polimaxx Polene 3342M Polypropylene Random Copolymer CHARACTERISTICS: HIGH CLARITY, GOOD FLOW, GOOD PROCESSABILITY APPLICATIONS: INJECTION MOLDING, INJECTION STRETCH BLOW MOLDING (ISBM) FOR FOOD CONTAINERS, BOTTLES, HOUSEWARES, CRATES |
|||
Processing Temperature | 190 - 230 °C | 374 - 446 °F | extrusion |
IRPC Polimaxx Polene HI830 Polystyrene APPLICATIONS: EXTRUSION APPLICATION, VACUUM SHEET : FOOD PACKAGING ELECTRICAL APPLIANCES, HOUSEHOLD PRODUCT, TOYS, SANITARY, etc. |
|||
Processing Temperature | 210 - 230 °C | 410 - 446 °F | C2 |
UBE 1026B1 Nylon 6 Homopolymer Film Specialties: Nucleated (High viscosity) Processing: T-die, Air blownApplications: General applicationsInformation provided by UBE. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 123-50W175 Thermoplastic Elastomer A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in thin wall .. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 201-73 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 273-40 Thermoplastic Elastomer A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 8211-25 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 8223-30M300 Thermoplastic Elastomer A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and .. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 8281-90MED Thermoplastic Elastomer A hard, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Processing Temperature | 180 - 230 °C | 356 - 446 °F | Barrel temperature |
Azoty Tarnow™ TARNOFORM 300 POM Basic, fast cycling injection molding grade suitable for many applications.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Processing Temperature | 180 - 230 °C | 356 - 446 °F | Barrel temperature |
Azoty Tarnow™ TARNOFORM 300 SI POM Tribological modified grade with silicon, for better sliding properties in plastic-plastic contact.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | Injection molding |
BASF Elastollan B 64 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | Injection molding |
BASF Elastollan B 90 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Processing Temperature | 200 - 230 °C | 392 - 446 °F | Injection |
Alliance Polymers Viprene™ G90A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G90A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Processing Temperature | 180 - 230 °C | 356 - 446 °F | Resin Temp. |
Beijing Chemical Industry KAIFA® GL1200 ABS General Purpose Grade Middle impact, Good mechanical strength, High flexural strengthInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Processing Temperature | 180 - 230 °C | 356 - 446 °F | Resin Temp. |
Beijing Chemical Industry KAIFA® GL2200 ABS Good Flow Grade High impact, Easy processingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Processing Temperature | 180 - 230 °C | 356 - 446 °F | Barrel temperature |
Azoty Tarnow™ TARNOFORM 200 LS POM Injection molding grade based on Tarnoform 200 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
BASF Elastollan 598 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and a high abrasion resistance.Typical Applications: Heel top-pieces, castor tyres and parts requiri.. |
|||
Processing Temperature | 180 - 230 °C | 356 - 446 °F | Resin Temp. |
Beijing Chemical Industry KAIFA® GL1300 ABS General Purpose Grade Excellent impact properties at low temperaturesInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Processing Temperature | 180 - 230 °C | 356 - 446 °F | Blow Molding |
Total Lumicene® mPE M 2710 EP Metallocene Polyethylene, Blown Film Lumicene® mPE M 2710 EP is a second generation metallocene based Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2710 EP can be processed at high output rates with low extrusion .. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 111-80 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 211-55 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 253-50W232 Thermoplastic Vulcanizate
(discontinued **) Product Description: A hard, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and is formulated to replace thermoset ru.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 221-87W211 Thermoplastic Elastomer
(discontinued **) A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |