Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 261-87 Thermoplastic Elastomer
(discontinued **) A hard, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance for use in wet electrical wire and cable applications. This gra.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Vyram™ 9201-85 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Processing Temperature | 190 - 230 °C | 374 - 446 °F | Barrel Temperature |
SABIC PP 6711K Polypropylene Copolymer for Injection Molding Product Description: PP 6711K is a controlled rheology grade with narrow molecular weight distribution intended specifically for producing injection molded articles with high clarity, good flow pro.. |
|||
Processing Temperature | 210 - 230 °C | 410 - 446 °F | Barrel Temperature |
SABIC PP 674K Polypropylene Copolymer for Injection Molding Product Description: PP 674K is specially developed for producing injection molded & ISBM articles with high clarity and also has better impact properties than homo PP counterparts.PP 674K has the .. |
|||
Processing Temperature | 177 - 230 °C | 350 - 446 °F | Average value: 199 °C Grade Count:8 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Processing Temperature | 160 - 230 °C | 320 - 446 °F | Membranes |
Lucobit Lucolit® 1321 Polyolefin TPO Granules, Blue Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi.. |
|||
Processing Temperature | 160 - 230 °C | 320 - 446 °F | Membranes |
Lucobit Lucobit® 1233 Ethylene Copolymer Bitumen Lucobit® combines the positive properties of polyolefins and bitumen. The material is black and consists of mixtures based on high quality polyethylene copolymers with varying additions of speci.. |
|||
Processing Temperature | 210 - 230 °C | 410 - 446 °F | |
Taiwan Sheen Soon Sheenthane® A9660 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 121-58W175 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for .. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 121-70B230 Thermoplastic Elastomer A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated to bond to sulfur or peroxide-cured thermoset EPDM rubber for corner .. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 201-64 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 273-40 Thermoplastic Elastomer A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 8211-35 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 8281-55MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 101-55 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Processing Temperature | 180 - 230 °C | 356 - 446 °F | Barrel temperature |
Azoty Tarnow™ TARNOFORM 300 GF2 POM 10% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Processing Temperature | 180 - 230 °C | 356 - 446 °F | Barrel temperature |
Azoty Tarnow™ TARNOFORM 300 GF6 BK POM 30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Processing Temperature | 180 - 230 °C | 356 - 446 °F | Barrel temperature |
Azoty Tarnow™ TARNOFORM 500 GF6 POM 30% glass fiber reinforced, high flow injection molding grade, suitable for applications where high strength and stiffness is required, combined with higher flowability during molding.Information pr.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | Injection molding |
BASF Elastollan 695 AU TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Processing Temperature | 200 - 230 °C | 392 - 446 °F | Injection |
Alliance Polymers Viprene™ G80A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G80A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Processing Temperature | 190 - 230 °C | 374 - 446 °F | Injection |
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Processing Temperature | 180 - 230 °C | 356 - 446 °F | Resin Temp. |
Beijing Chemical Industry KAIFA® GL2200 ABS Good Flow Grade High impact, Easy processingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Vyram™ 9201-75 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Processing Temperature | 177 - 230 °C | 350 - 446 °F | Average value: 199 °C Grade Count:24 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Geolast® 701-70 Thermoplastic Elastomer A soft, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Geolast® 703-45 Thermoplastic Elastomer A hard, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 8211-60 Thermoplastic Elastomer
(discontinued **) A soft, colorable, non-hygroscopic, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance .. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 101-60W261 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Processing Temperature | 185 - 230 °C | 365 - 446 °F | Metering Zone |
Wacker Silicones Geniomer® 60 Silicone TPE SLM TPSE 60 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer Product Description: A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for.. |