Polymer Property : Processing Temperature = 1000 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 540 °C
1000 °F
Typical Firing Temperature
Ferro IP 530 Thick Film Glass
Glass Type: Pb-Si-B-Al Typical Powder Form: RWG Typical Application: General Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conducto..