Processing Temperature 103 °C
218 °F
Hot Forming Temperature
Spartech Polycast Poly 2000 (Mil-P-25690;Class 1) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Processing Temperature 103 °C
218 °F
Hot Forming Temperature
Spartech Polycast Poly 2000 (Mil-P-25690;Class 2) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.