Polymer Property : Processing Temperature = 1050 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 1050 °C
1920 °F
fusing temperature
Wall Colmonoy COLMONOY® 75 - Nickel-Chromium-Tungsten-Boron Matrix Alloy
Description and Application: A nickel-chromium-boron matrix alloy rich in chromium boride holds extremely hard tungsten-carbide particles. Used primarily for protection from severe sliding abrasion..
Processing Temperature 1050 °C
1920 °F
hardening temperature, then quenched in air and tempered 2 + 2 h at 1070°F (hardness = 56 HRC)
Bohler-Uddeholm UDDEHOLM HOTVAR® Hot Work Tool Steel
Molybdenum-vanadium alloyed steelHotvar® is a premium hot work steel developed by Uddeholm to provide very good performance in tooling up to 1200°F (650°C). The alloying elements in Hotvar® are ..