Processing Properties Metric English Comments
Processing Temperature 1020 - 1050 °C
1870 - 1920 °F
Hardened then air cooled
Misumi DC53 JIS Tool Steel
General purpose cold work die and mold steel whose strength and toughness approach those of high speed steels. Good machinability and grindability. Tougher than D2 Tool Steel. Machines 30% faster th..