Processing Temperature 575 °C
1070 °F
Typical Firing Temperature
Ferro EG 2964 Glaze and Sealant Glass
Glass Type: Bi-Zn-B Typical Powder Form: VWG Typical Application: ZnO, Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and ins..