Polymer Property : Processing Temperature = 1120 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 571 - 604 °C
1060 - 1120 °F
Brazing Range
Lucas-Milhaupt AL 716 Aluminum Brazing Filler Metal
Applications:AL 716 filler metal is generally used to join aluminum and aluminum alloys. It can be used to join titanium or aluminum to dissimilar metals. When joining to dissimilar metals thought..
Processing Temperature 582 - 604 °C
1080 - 1120 °F
Brazing Range
Lucas-Milhaupt AL 718 Aluminum Brazing Filler Metal
Applications:AL 718 filler metal is generally used to join aluminum and aluminum alloys. It can be used to join titanium or aluminum to dissimilar metals. When joining to dissimilar metals thought..