Polymer Property : Processing Temperature = 1140 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 1140 °C
2080 °F
fusing temperature
Wall Colmonoy WALLEX 40 Cobalt-Nickel Alloy
Description: A cobalt-nickel alloy powder that forms deposits similar to those of Wallex 50, but softer. Finished with carbide tools and grinding.Methods of Application: Spraywelder, Fusewelder, PT..