Processing Properties Metric English Comments
Processing Temperature 670 °C
1240 °F
Typical Firing Temperature; Typical Firing Time: 5-10 min.
Ferro IX 2218 Passivation Glasses - High Voltage (Zn-B-Silicates)
Typical Powder Form: REG, MVG Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures a..