Processing Properties Metric English Comments
Processing Temperature 54.0 - 82.0 °C

@Time 900 sec
129 - 180 °F

@Time 0.250 hour
Immersion
Henkel Turco Ridoline 909 Cleaner
Turco Ridoline 909 is a medium-duty, caustic-free, immersion cleaner that provides excellent wetting, emulsifying and dispersing properties which are effective in the removal of a wide variety of so..
Processing Temperature 54.0 °C
129 °F
Roll 2 Temperature
SK Chemicals SKYGREEN® PETG 2008 Specially Formulated PET Copolymer Resin
SKYGREEN PETG is an amorphous copolyester in which a certain amount of ethylene glycol is replaced with 1,4-cyclohexane dimethanol (CHDM), which prevent crystallization, leading to improved processa..
Processing Temperature 54.0 - 82.0 °C

@Time 900 sec
129 - 180 °F

@Time 0.250 hour
Immersion
Henkel Ridoline 298 Cleaner
Ridoline 298 is a liquid, non-silicated, immersion cleaner for aluminum and aluminum alloys. It is formulated for use in anodizing and conversion coating lines. It is free rinsing and will remove a ..