Processing Properties Metric English Comments
Processing Temperature 635.0 - 746.1 °C
1175 - 1375 °F
Brazing Range
Lucas-Milhaupt EASY FLO Silver Based Cadmium-Bearing Filler Metal
Applications: Easy-Flo is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wettin..