Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 857.2 - 1010 °C | 1575 - 1850 °F | Brazing Range |
Lucas-Milhaupt BRAZE 630 Silver Based Cadmium Free Filler Metal Characteristics: Braze 630 is very sluggish because of its wide melting range, and will bridge wide or irregular joint clearances. To avoid liquation (separation and flow of the low-melting compon.. |
|||
Processing Temperature | 857.2 - 968.3 °C | 1575 - 1775 °F | Brazing Temperature |
Lucas-Milhaupt Silvaloy® A54N Brazing Alloy Silvaloy A54N is a silver brazing alloy suitable for furnace brazing due to its low zinc content. Its broader melting range is helpful where clearances are not uniform. During melting, Silvaloy A54N.. |