Processing Temperature 971 - 1040 °C
1780 - 1900 °F
Brazing Range
Lucas-Milhaupt BRAZE 852 Silver Based Cadmium Free Filler Metal
Characteristics: Braze 852 is a high temperature, free flowing silver brazing filler metal usable both for torch and atmosphere furnace brazing. Due to the high flow point of this alloy, torch brazi..