Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 101 °C | 214 °F | Seal Initiation temperature |
Dow Elite® 5100 Linear Low Density Polyethylene 5100 enhanced polyethylene resin is a copolymer produced via INSITE Technology from Dow Plastics. It offers extremely high impact resistance, combined with excellent tear, tensile, and puncture pro.. |