Processing Properties Metric English Comments
Processing Temperature 143 - 287 °C
289 - 549 °F
Injection
Dyna-Purge® K Purging Compound
Designed or a broad range of "Low-Temp" resinsGeneral Description:DYNA-PURGE K is a low-temp, non-abrasive, non-chemical “engineered” thermoplastic purging compound, formulated to flow nat..
Processing Temperature 143 - 287 °C
289 - 549 °F
Extrusion
Dyna-Purge® K Purging Compound
Designed or a broad range of "Low-Temp" resinsGeneral Description:DYNA-PURGE K is a low-temp, non-abrasive, non-chemical “engineered” thermoplastic purging compound, formulated to flow nat..
Processing Temperature 143 °C
289 °F
Ashley Polymers Ashlene® ABS Resin R2018, 18% Glass Reinforced
General purpose, 18% glass reinforced ABS resin.Data provided by the manufacturer
Processing Temperature 143 - 160 °C
289 - 320 °F
Average value: 156 °C Grade Count:4
Overview of materials for Acrylic, Optical Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr..