Polymer Property : Processing Temperature = 38.0 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 4.00 - 38.0 °C
39.2 - 100 °F
Surface temperature
BASF Master Builders Solutions ChemRex® CX-943 Squeegee-grade Polyurethane Adhesive  (discontinued **)
CX-943 is a one-component polyurethane-based squeegee-grade, structural adhesive. Its elastomeric properties enable it to move with substrates as it expands and contracts. The patented formula is ..
Processing Temperature 23.0 - 38.0 °C
73.4 - 100 °F
Henkel Alodine 1200S Conversion Coating
Alodine 1200S is a powdered chemical used to produce a protective coating on aluminum to minimize corrosion and provide an improved bond for paint. Alodine 1200S coating chemical, listed on Qualifie..
Processing Temperature 23.0 - 38.0 °C
73.4 - 100 °F
Henkel Turco Alodine 1201 Touch-Up Conversion Coating
Alodine 1201 is a nonflammable, chromic acid-based coating chemical that will produce a chrome conversion coating on aluminum and its alloys.
Processing Temperature 21.0 - 38.0 °C
69.8 - 100 °F
Henkel Turco Metal Glo #6 Jet Metal Brightener
Turco Metal Glo #6 is a nonflammable, tri-acid, detergent-solvent based cleaner, brightener, deoxidizer and prepaint conditioner for aluminum. It contains viscosity builders that allow for added con..