Processing Temperature 454 - 468 °C
850 - 875 °F
Brazing Range
Lucas-Milhaupt AL 815 Aluminum Brazing Filler Metal
Characteristics:AL 815 is a general purpose free flowing soldering filler metals for use with all solderable aluminum and aluminum alloys when soldering with torch. Information provided by Lucas-Mi..