Processing Temperature <= 243 °C
<= 469 °F
Ineos Nova Zylar® 220 High Performance Styrenic, Acrylic Copolymer  (discontinued **)
Excellent moldability, High clarity, Extended toughness and elongation, meets USP XXI specification for Class VI Plastics, Property retention after gamma irradiationApplications: Display, medical de..