Processing Properties Metric English Comments
Processing Temperature 379 - 429 °C
714 - 804 °F
Average value: 404 °C Grade Count:13
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum..