Processing Properties Metric English Comments
Processing Temperature 738 - 871 °C
1360 - 1600 °F
Brazing Temperature
Lucas-Milhaupt Silvaloy® A25T Brazing Alloy
Silvaloy A25T is an economical filler metal for ferrous and nonferrous joints not requiring high ductility or impact strength. It is similar to Silvaloy A40T, however flow is less active and tempera..