Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 900 °C | 1650 °F | Typical Firing Temperature |
Ferro EG 0024 Specialty Glass Glass Type: Si-B-MG-Al Typical Powder Form: VWG Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-ph.. |
|||
Processing Temperature | 900 °C | 1650 °F | Typical Firing Temperature |
Ferro EG 0026 Glaze and Sealant Glass Glass Type: Ca-B-Al-Si Typical Powder Form: MVG Typical Application: Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insul.. |
|||
Processing Temperature | 900 °C | 1650 °F | Typical Firing Temperature |
Ferro EG 2778 Thick Film Glass Glass Type: Si-Al-Ca Typical Powder Form: MVG Typical Application: Dielectric Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conduct.. |
|||
Processing Temperature | 900 °C | 1650 °F | Typical Firing Temperature |
Ferro F 2719 Metal Sealing Glass Type: Si-Ba Alkali Typical Powder Form: VSD Typical Application: Kovar Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals.. |