Ejection Temperature 100 °C
212 °F
Covestro Bayblend® FR 3000 Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradeeasy-flow gradeVicat/B 120 temperature = 97 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (2.0 mm)no j..
Ejection Temperature 100 °C
212 °F
Covestro Bayblend® FR 3002 Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradefor notebooks and thinwall applicationsVicat/B 120 temperature = 99 °CUL-listing 94 V-0 (1.2 mm)antimony- chlorine- and bromine-free flame retardantglow wire test (GWFI): 960..
Ejection Temperature 100 °C
212 °F
Covestro Bayblend® FR 3005 HF Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradevery easy-flow gradeVicat/B 120 temperature = 96 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantPreprocessingMax. Water content
Ejection Temperature 100 °C
212 °F
Covestro Bayblend® FR 3005 Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradeeasy-flow gradeVicat/B 120 temperature = 95 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (2.0 mm)no j..