Polymer Property : Ejection Temperature = 307 °F
Polymer Property :
Ejection Temperature =
307 °F
Product List
Processing Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties
Metric
English
Comments
Ejection Temperature
153
°C
307
°F
Covestro Apec® 1795 Polycarbonate
Easy flowingeasy to demoldsoftening temperature (VST/B 120)=173°CPreprocessingMax. Water content