Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 130.0 - 140.0 MPa | 18850 - 20310 psi | |
Premix Thermoplastics PRE-ELEC® PBT 1455 PRE-ELEC PBT 1455 is a conductive thermoplastic compound based on PBT. Conductivity is achieved by using special conductive carbon black. PRE-ELEC PBT 1455 has excellent mechanical properties as wel.. |