Polymer Property : Injection Pressure = 175 psi
Polymer Property :
Injection Pressure =
175 psi
Product List
Processing Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties
Metric
English
Comments
Injection Pressure
1.21
-
1.55
MPa
175
-
225
psi
Secondary
Clariant Renol PCSP0011 Polycarbonate Alloy, Glass Fiber and Glass Bead Filled
Data provided by Clariant Masterbatches