Processing Properties Metric English Comments
Injection Pressure 3.40 - 10.3 MPa
493 - 1490 psi
Injection Molding
Stellarchem SE/PA745B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..